Main ingredients: Pure MDI and polymerized MDI. Manufactured by Kumho, Korea. Used for thermal insulation, soundproofing, and vibration damping applications...
0 ₫
Main ingredients: Pure MDI and polymerized MDI.
Manufactured by Tosoh, Japan.
Packaging: 250kg/drum.
Each drum volume: 250L.
Color: Blue drum...
0 ₫
Main ingredients: Pure MDI and polymerized MDI.
Manufactured by Wanhua Chemical Group, China.
Each drum volume: 250L.
Packaging: 250kg/drum.
Color:...
0 ₫
Cream time: 6–7 seconds
String time: 28–35 seconds
Free rise density: 12.5–13.5 kg/m³
Hardness: 45
Mixing ratio: POLYOL 100, ISO 120–150...
0 ₫
Key features:
Cream time: 33 seconds
Rise time: 34 seconds
String time: 130 seconds
Mixing ratio: POLYOL 1, ISO 1–1.1...
0 ₫
Cream time: 25 seconds
Rise time: 27 seconds
String time: 60 seconds
Mixing ratio: POLYOL 1, ISO 1–1.1...
0 ₫