Main ingredients: Pure MDI and polymerized MDI. Manufactured by Kumho, Korea. Used for thermal insulation, soundproofing, and vibration damping applications...
Main ingredients: Pure MDI and polymerized MDI. Manufactured by Tosoh, Japan. Packaging: 250kg/drum. Each drum volume: 250L. Color: Blue drum...
Main ingredients: Pure MDI and polymerized MDI. Manufactured by Wanhua Chemical Group, China. Each drum volume: 250L. Packaging: 250kg/drum. Color:...
Cream time: 6–7 seconds String time: 28–35 seconds Free rise density: 12.5–13.5 kg/m³ Hardness: 45 Mixing ratio: POLYOL 100, ISO 120–150...
Key features: Cream time: 33 seconds Rise time: 34 seconds String time: 130 seconds Mixing ratio: POLYOL 1, ISO 1–1.1...
Cream time: 25 seconds Rise time: 27 seconds String time: 60 seconds Mixing ratio: POLYOL 1, ISO 1–1.1...